Acta Marisiensis.
Seria Technologica



ISSN 2668-4217
ISSN-L 2668-4217
(Online)


Română

HomeEditorial boardSubmit paperPublication ethicsContactIndexing
Year 2023
Volume 20 (XXXVII), no 1
Volume 20 (XXXVII), no 2

Year 2022
Volume 19 (XXXVI), no 1
Volume 19 (XXXVI), no 2

Year 2021
Volume 18 (XXXV), no 1
Volume 18 (XXXV), no 2

Year 2020
Volume 17 (XXXIV), no 1
Volume 17 (XXXIV), no 2

Year 2019
Volume 16 (XXXIII), no 1
Volume 16 (XXXIII), no 2

Year 2018
Volume 15 (XXXII), no 1
Volume 15 (XXXII), no 2

Year 2017
Volume 14 (XXXI), no 1
Volume 14 (XXXI), no 2

Year 2016
Volume 13 (XXX), no 1
Volume 13 (XXX), no 2

Year 2015
Volume 12 (XXIX), no 1
Volume 12 (XXIX), no 2

Year 2014
Volume 11 (XXVIII), no 1
Volume 11 (XXVIII), no 2

Year 2013
Volume 10 (XXVII), no 1
Volume 10 (XXVII), no 2

Year 2012
Volume 9 (XXVI), no 1
Volume 9 (XXVI), no 2

Year 2011
Volume 8 (XXV), no 1
Volume 8 (XXV), no 2

Year 2010
Volume 7 (XXIV), no 1
Volume 7 (XXIV), no 2

Year 2009
Volume 6 (XXIII)

2023, Volume 20 (XXXVII), no 2

Obtaining and Characterizing the Dielectric and Ferroelectric Properties of the PZT-PMS Complex System through Solid State Reactions and Spark Plasma Sintering

Author(s):
Alina Iulia DUMITRU, National Institute for Research & Development in Electrical Engineering ICPE-CA, Bucharest, Romania, Valahia University from Targoviste, Doctoral School of Materials Engineering, Targoviste, Romania
Dorinel TALPEANU, National Institute for Research & Development in Electrical Engineering ICPE-CA, Bucharest, Romania
Rodica Mariana ION, National Institute for Research and Development in Chemistry and Petrochemistry - ICECHIM, Bucharest, Romania
Ildiko PETER, „George Emil Palade” University of Medicine, Pharmacy, Science and Technology of Targu Mures, Romania

Abstract:
In this paper B-oxide sintering process and Spark plasma Sintering (SPS) method is used to synthesize 0.88Pb(Zr0.52Ti0.48)O3 – 0.12Pb(Mn1/3Sb2/3)O3 – x at%Pr complex system where x = 0 and 0.02. The sintering temperature used in the SPS technique is considerably lower than that used in the B-oxide method (200 to 400 oC) with significant decrease of the duration of the sintering route, arriving to some minutes instead of some hours.
The aim of the study is the investigation of the effect of sintering technique on the dielectric and ferroelectric properties of such piezoelectric materials. The properties of the developed ceramic materials were determined: the development of crystalline phases was investigated by X-ray diffraction technique and the microstructural behavior by scanning electron microscopy was observed. The composition obtained by the SPS technique shows a lower remnant polarization and maximum strain, as well as a higher coercive field, compared to the those obtained using the same composition produced by B-oxide method.

DOI: https://doi.org/10.2478/amset-2023-0010

Pages: 1-7